| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
| 基本性能 | 吸水率 | ASTM D-570 | 0.01> | % | |
| 线性模压收缩率 | KPIC Method | 1.4-1.8 | % | ||
| 熔体流动速率 | ASTM D-1238 | 10 | g/10min | ||
| 密度 | ASTM D-1505 | 0.91 | g/cm3 | ||
| 机械性能 | 弯曲模量 | ASTM D-790 | 18,000 | ||
| 抗张强度(屈服) | ASTM D-638 | 330 | |||
| 断裂伸长率 | ASTM D-638 | 200< | % | ||
| Izod冲击强度(缺口) | ASTM D-256 | 10 | |||
| 介电强度 | Short Time | ASTM D-149 | 40 | KV/M | |
| 洛氏硬度 | ASTM D-785 | 102 | R Scale | ||
| 电气性能 | 介电常数 | 1KHz | ASTM D-150 | 2.3 | |
| 耗散(损耗)因数 | 1KHz | ASTM D-150 | 2 | ||
| 耐电弧性 | ASTM D-495 | 130 | sec. | ||
| 体积电阻率 | ASTM D-257 | 1 | 1017ohm.H | ||
| 热性能 | 热膨胀系数(线性) | ASTM D-696 | 10 | 10-5H/H℃ | |
| 维卡软化点 | ASTM D-1525 | 153 | ℃ | ||
| 热传导性 | KPIC Method | 3 | |||
| 热变形温度 | ASTM D-648 | 135 | ℃ | ||
| 比热 | KPIC Method | 0.46 | ℃ | ||